RaggedEdge 04-25-2009 06:38 AM


Originally Posted by James (Post 2839669)
..... for below water application apply immersion rated epoxy, apply immersion rated topcoats per spec. If the boat does not stay in the water more than 7 days @ 77 degrees (as a rule of thumb) then a conventional aliphatic urethane, also knows as "single stage", to include all brands and brand names "Imron" etc... will work. If you keep the boat in the water it is a different game -



Do I follow you here, a rated epoxie primer followed by the rated paint?

Where could you get immersion rated paints? Do manufacturers such as DuPont, PPG, or others have them? Or are they specialty companies?

verbi69 05-06-2009 10:57 AM

There are many paint manufacturers that have "immersion" quality primer and paints. Don't be scared of the word "rated".
"good for" could be substituted.......lol!!
ICI Devoe, International Paints, along with many others have several Heavy Industrial submersible paints available.....that perform well under constant submersion.....stay away from the spray bombs.

verbi69 05-06-2009 11:01 AM

And the other thing to remember is to never topcoat epoxy primer with a single stage paint...there is not enough strength in single stage paint to adhere to 2-part epoxies.

Strip Poker 388 05-09-2009 04:50 PM


Originally Posted by daredevil (Post 2772477)
Yep,,,,150 gritt and go !!!!!!!!!!!!


What about 320? it make it look better