If you're running in salt water a lot and the aluminum parts are not coated or anodized, consider using Tef-Gel in between the bolt and the part. Aluminum and stainless are at opposite ends of the galvanic scale and will corrode together very badly in the presence of salt water. By "badly", I mean that they will virtually weld themselves together...
|