R-hand rotation bravo 28. Casting defect on the barrel of the prop. I suspect this would affect the flow dynamics along the leading edge of the blade. Can this defect be repaired correctly? If not, any idea if Mercury would likely replace it without a big hassle?
Attached Thumbnails Bravo casting defect-bravo-28-001.jpg   Bravo casting defect-bravo-28-005.jpg   Bravo casting defect-bravo-28-003.jpg  


Last edited by RedDog382; 12-03-2005 at 01:52 PM.
RedDog382 is offline  
Reply
Old 12-03-2005 | 06:04 PM
  #2  
LAKESIDE RESTORATIONS's Avatar
Lakeside Restorations.com
 
Joined: Nov 2003
Posts: 2,512
Likes: 2
From: NorthEastern, PA
Default Re: Bravo casting defect

Originally Posted by RedDog382
R-hand rotation bravo 28. Casting defect on the barrel of the prop. I suspect this would affect the flow dynamics along the leading edge of the blade. Can this defect be repaired correctly? If not, any idea if Mercury would likely replace it without a big hassle?
It probably could be fixed by a reputable prop shop. Operative word being reputable. However If the prop is new & you bought it from a Merc dealer, I would call them & see what they or merc will do for you. They may or may not be able to help you, As I always say it doesnt hurt to ask the worst they could say is no. Good luck with your prop situation.. Look on the bright side of the bad current scenario, its only a prop not an engine or drive... Jamie
www.LakesideRestorations.com
__________________
www.LakesideRestorations.com 570-639-2628
We Make Fast Toys Faster, Cool Toys Cooler and Old Toys New!.. Performance, Custom & OEM Parts & much MORE![/CENTER]
LAKESIDE RESTORATIONS is offline  
Reply
Old 12-04-2005 | 10:49 AM
  #3  
throttleup's Avatar
Registered
 
Joined: Mar 2002
Posts: 5,143
Likes: 1
From: Cajun Country
Default Re: Bravo casting defect

It is not a big deal to repair the prop and make it look as if it had never been repaired.

If the prop is still stock and has had no repairs done in the past I would contact Mercury and see if they will repair of replace the prop for you at no charge. The Warranty is good for one year from the date of purchase, or 90 days if used on "high performance equipment".

Matt
throttleup is offline  
Reply
Old 12-04-2005 | 11:53 AM
  #4  
bbladesprops's Avatar
Offshoreonly Advertiser
20 Year Member
Offshoreonly Advertiser
 
Joined: Jun 2003
Posts: 3,878
Likes: 47
From: Princeton, Wisconsin
Default Re: Bravo casting defect

If you have a receipt for the prop or the boat that it was part of, the selling dealer can ship it back within 1 year of purchase for a credit to his account. Then the dealer replaces the propeller. If that doesn't work, you may want to call Mercury customer service for their input.

920-929-5040
__________________
Brett Anderson / BBLADES Professional Propellers
920-295-4435 http://www.bblades.com/
[email protected]
bbladesprops is offline  
Reply
Related Topics
Thread
Thread Starter
Forum
Replies
Last Post
sun28
General Q & A
5
06-08-2012 08:17 AM
Griswald
General Q & A
6
02-11-2008 07:14 AM
Interceptor
Fountain
0
11-07-2006 06:29 AM
Grog
General Q & A
2
02-22-2005 02:57 PM
mtm
General Q & A
13
12-26-2004 02:50 PM

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Contact Us - Archive - Advertising - Cookie Policy - Privacy Statement - Terms of Service

Copyright © 2026 MH Sub I, LLC dba Internet Brands. All rights reserved. Use of this site indicates your consent to the Terms of Use.